Abubuwan Sinadarai (%)CuNi44
| Ni | Mn | Fe | Si | Cu | Wani | Umarnin ROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 44 | 1.50% | 0.5 | - | Bal | - | ND | ND | ND | ND |
Kayayyakin InjiCuNi44
| Matsakaicin Yanayin Sabis na Ci gaba | 400 ºC |
| Juriyar yanayi a 20ºC | 0.49 ± 5% ohm*mm2/m |
| Yawan yawa | 8.9 g/cm3 |
| Ma'aunin Juriya na Zafin Jiki | < -6 × 10-6/ºC |
| EMF VS Cu (0~100ºC) | -43 μV/ºC |
| Wurin narkewa | 1280 ºC |
| Ƙarfin Taurin Kai | Min 420 Mpa |
| Ƙarawa | Mafi ƙarancin 25% |
| Tsarin Micrographic | Austenite |
| Kadarar Magnetic | A'a. |
Siffofin samfurin:
1) Kyakkyawan ƙarfin hana iskar shaka da ƙarfin injiniya a babban zafin jiki;
2) Babban juriya da ƙarancin zafin jiki na juriya;
3) Kyakkyawan aiki mai kyau da kuma sauƙin sarrafawa;
4) Kyakkyawan aikin walda