Bar Ni35Cr20 6mm Ba Magnetic Ba don Ƙarfin Ƙimar Wutar Lantarki

Takaitaccen Bayani:

NiCr 35 20 (1.4860) ana iya amfani dashi a yanayin aiki har zuwa 1000°C. Nickel-chromium alloy 35/20 an kwatanta shi da babban juriya da ƙarancin farashi idan aka kwatanta da sauran gami da nickel-chromium. Duk da babban abun ciki na baƙin ƙarfe, NiCr3520 yana da juriya ga oxidation da lalata sinadarai. Nichrome 35/20 ba Magnetic bane.


  • Daraja:Ni30Cr20
  • Girman:6mm ku
  • Alamar:Tanki
  • Siffar:mashaya
  • Girma (g/cm³):7.9
  • Abubuwan Magnetic:ba
  • Cikakken Bayani

    FAQ

    Tags samfurin

         NiCr 35 20 (1.4860) ana amfani dashi azaman kayan lantarki a cikin kayan gida da sauran kayan dumama lantarki. Yana da kyau ductility bayan dogon lokaci amfani, mai kyau inji dukiya a high zafin jiki da kuma mai kyau weldability. Matsakaicin zafin aiki a cikin iska shine +600°C lokacin amfani da wayoyi juriya da +1050°C lokacin amfani da dumama wayoyi.

    • high-darajar lantarki resistors da kuma dumama wayoyi.
    • abubuwan dumama wutar lantarki (Barguna na lantarki da pads, kujerun mota, na'urar dumama allo, dumama bene, resistors).
    • murhun masana'antu har zuwa 1000 °
    • dumama igiyoyi, igiya dumama dumama igiya heaters a defrosting da kuma de-kankara abubuwa
    Daraja Ni80Cr20 Ni70Cr30 Ni60Cr23 Ni60Cr15 Ni35Cr20 Karma Evanohm
    Abun ƙima% Ni Bal Bal 58.0-63.0 55.0-61.0 34.0-37.0 Bal Bal
      Cr 20.0-23.0 28.0-31.0 21.0-25.0 15.0-18.0 18.0-21.0 19.0-21.5 19.0-21.5
      Fe ≦1.0 ≦1.0 Bal Bal Bal 2.0-3.0 -
            Al1.0-1.7 Ti 0.3-0.5     Al2.7-3.2 Mn0.5-1.5 Al2.7-3.2 Cu2.0-3.0 Mn0.5-1.5
    Matsakaicin zafin aiki (°C) 1200 1250 1150 1150 1100 300 400
    Resisivity(Ω/cmf,20℃) 1.09 1.18 1.21 1.11 1.04 1.33 1.33
    Resisivity(uΩ/m,60°F) 655 704 727 668 626 800 800
    Girma (g/cm³) 8.4 8.1 8.4 8.2 7.9 8.1 8.1
    Ƙarfafa Ƙarfafawa (KJ/m·h·℃) 60.3 45.2 45.2 45.2 43.8 46.0 46.0
    Ƙididdigar Faɗaɗɗen Layi (×10n6/ ℃) 20-1000 ℃) 18.0 17.0 17.0 17.0 19.0 - -
    Wurin narkewa (℃) 1400 1380 1370 1390 1390 1400 1400
    Hardness (Hv) 180 185 185 180 180 180 180
    Ƙarfin Ƙarfi (N/mm2 ) 750 875 800 750 750 780 780
    Tsawaita(%) ≥20 ≥20 ≥20 ≥20 ≥20 10-20 10-20
    Tsarin Micrographic Austenite Austenite Austenite Austenite Austenite Austenite Austenite
    Abubuwan Magnetic Ba Ba Ba Dan kadan Ba Ba Ba
    Rayuwa mai sauri (h/℃) ≥81/1200 ≥50/1250 ≥81/1200 ≥81/1200 ≥81/1200 - -

     