Bayanin Samfura
Waɗannan wayoyi masu juriya an yi amfani da su sosai don daidaitattun resistors, mota
sassa, iska resistors, da dai sauransu ta yin amfani da insulation aiki mafi dacewa da wadannan aikace-aikace, shan cikakken amfani da musamman fasali na enamel shafi.
Bugu da ƙari kuma, za mu gudanar da wani enamel rufi rufi na daraja karfe waya kamar azurfa da platinum waya bisa oda. Da fatan za a yi amfani da wannan samarwa-kan-oda.
Tpye na Insulation:
1) Polyester juriya waya, class 130
2) Modified polyester juriya waya, class 155
3) Polyesteramide juriya waya, class 180
4) Polyester (imide) mai rufi da polyamide-imide juriya waya, aji 200
5) Polyimide juriya waya, aji 220
Constantan 6J40 | Sabon Constantan | Manganin | Manganin | Manganin | ||
6j11 | 6j12 | 6 j8 | 6j13 | |||
Babban Sinadaran % | Mn | 1 ~ 2 | 10.5 ~ 12.5 | 11-13 | 8 ~ 10 | 11-13 |
Ni | 39-41 | - | 2 ~ 3 | - | 2 ~ 5 | |
Cu | REST | REST | REST | REST | REST | |
Al2.5 ~ 4.5 Fe1.0 ~ 1.6 | Si1~2 | |||||
Matsakaicin Zazzabi don Abubuwan Haɓaka | 5 ~ 500 | 5 ~ 500 | 5 ~ 45 | 10 ~ 80 | 10 ~ 80 | |
Yawan yawa | 8.88 | 8 | 8.44 | 8.7 | 8.4 | |
g/cm3 | ||||||
Resistivity | 0.48 | 0.49 | 0.47 | 0.35 | 0.44 | |
μΩ.m, 20 | ± 0.03 | ± 0.03 | ± 0.03 | ± 0.05 | ± 0.04 | |
Ƙarfafawa | ≥15 | ≥15 | ≥15 | ≥15 | ≥15 | |
% % 0.5 | ||||||
Juriya | -40-40 | -80 ~ + 80 | -3-+20 | -5-+10 | 0 ~ +40 | |
Zazzabi | ||||||
Quotiety | ||||||
α,10 -6 / | ||||||
Thermoelectromotive | 45 | 2 | 1 | 2 | 2 | |
karfi zuwa Copper | ||||||
μv / (0 ~ 100) |
Tpye na Bare Waya
babba dukiya nau'in | Kuni1 | KUNI2 | KUNI6 | KUNI10 | KuNi19 | KuNi23 | KuNi30 | KuNi34 | KUNI44 | |
babba sinadaran abun da ke ciki | Ni | 1 | 2 | 6 | 10 | 19 | 23 | 30 | 34 | 44 |
MN | / | / | / | / | 0.5 | 0.5 | 1.0 | 1.0 | 1.0 | |
CU | hutawa | hutawa | hutawa | hutawa | hutawa | hutawa | hutawa | hutawa | hutawa | |
max aiki zafin jiki | / | 200 | 220 | 250 | 300 | 300 | 350 | 350 | 400 | |
yawa g/cm3 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | |
resistivity da 20 °c | 0.03 ± 10% | 0.05 ± 10% | 0.1 ± 10% | 0.15 ± 10% | 0.25 ± 5% | 0.3 ± 5% | 0.35 ± 5% | 0.40 ± 5% | 0.49 ± 5% | |
zafin jiki coefficient na juriya | <100 | <120 | <60 | <50 | <25 | <16 | <10 | -0 | <-6 | |
tensile karfin mpa | >210 | >220 | >250 | >290 | >340 | >350 | >400 | >400 | >420 | |
elongation | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 | |
narkewa batu °c | 1085 | 1090 | 1095 | 1100 | 1135 | 1150 | 1170 | 1180 | 1280 | |
coefficient na rashin daidaituwa | 145 | 130 | 92 | 59 | 38 | 33 | 27 | 25 | 23 |