Barka da zuwa gidajen yanar gizon mu!

Soft Magnetic Alloy Waya Ni77mo4cu5

Takaitaccen Bayani:

(Magnetic alloy mai laushi)

Ni77mo4cu5 nickel-iron Magnetic Alloy, tare da kusan 80% nickel da 20% baƙin ƙarfe. An ƙirƙira shi a cikin 1914 ta masanin kimiyyar lissafi Gustav Elmen a dakunan gwaje-gwaje na wayar tarho, sananne ne saboda ƙarfin ƙarfin maganadisu sosai, wanda ya sa ya zama mai amfani a matsayin kayan masarufi a cikin kayan lantarki da na lantarki, da kuma garkuwar maganadisu don toshe filayen maganadisu. Kayayyakin permalloy na kasuwanci yawanci suna da alaƙar dangi kusan 100,000, idan aka kwatanta da dubu da yawa don ƙarfe na yau da kullun.
Bugu da kari ga babban permeability, sauran Magnetic kaddarorin su ne low coercivity, kusa da sifili magnetostriction, da kuma gagarumin anisotropic magnetoresistance. Ƙananan magnetostriction yana da mahimmanci ga aikace-aikacen masana'antu, yana ba da damar yin amfani da shi a cikin fina-finai na bakin ciki inda damuwa mai canzawa zai haifar da babban bambanci a cikin abubuwan maganadisu. Resistance wutar lantarki na Permalloy na iya bambanta kamar 5% ya danganta da ƙarfi da alkiblar filin maganadisu. Permalloys yawanci suna da tsari mai siffar cubic crystal a tsakiya tare da tsaka-tsakin tsayin daka na kusan 0.355 nm a cikin kusancin tarin nickel na 80%. Rashin lahani na permalloy shine cewa ba shi da ductile ko aiki, don haka aikace-aikacen da ke buƙatar cikakkun siffofi, irin su garkuwar maganadisu, an yi su da wasu manyan abubuwan haɓakawa kamar mu karfe. Ana amfani da Permalloy a cikin laminations masu canzawa da shugabannin rikodin maganadisu.
Ni77mo4cu5 ana amfani dashi ko'ina a masana'antar rediyo-lantarki, kayan aiki daidai, sarrafa nesa da tsarin sarrafawa ta atomatik.


  • Samfurin NO:Ni77mo4cu5
  • Matsayi:Mai haske
  • Juriya:0.55
  • Ƙimar faɗaɗa madaidaiciya (20ºC ~ 200ºC)X10-6/ºC: 25
  • Yawan yawa (g/cm3):8.6
  • Matsayin Curie Tc/ºC:350
  • Asalin:China
  • Cikakken Bayani

    FAQ

    Tags samfurin

    Na yau da kullun%

    Ni 75.5-78 Fe Bal. Mn 0.3 ~ 0.6 Si 0.15 ~ 0.3
    Mo 3.9 ~ 4.5 Cu 4.8 ~ 6.0
    C ≤0.03 P ≤0.02 S ≤0.02

    Hannun kayan aikin injiniya

    Ƙarfin bayarwa Ƙarfin Ƙarfi Tsawaitawa
    Mpa Mpa %
    980 980 2 ~ 40

    Abubuwan dabi'un Jiki na yau da kullun

    Yawan yawa (g/cm3) 8.6
    Rashin ƙarfin lantarki a 20ºC (Om * mm2/m) 0.55
    Ƙimar faɗaɗa madaidaiciya (20ºC ~ 200ºC) X10-6/ºC 10.3 ~ 11.5
    Saturation magnetostriction coefficient λθ/ 10-6 2.4
    Matsayin Curie Tc/ºC 350

     

    The Magnetic Properties na gami da high permeability a cikin rauni filayen
    1 j77 Halin farko Matsakaicin iyawa Tilastawa Saturation Magnetic Induction tsanani
    Fati mai birgima mai sanyi / takarda.
    Kauri, mm
    μ0.08/ (mH/m) μm/ (mH/m) Hc/ (A/m) BS/T
    0.01 mm 17.5 87.5 5.6 0.75
    0.1 ~ 0.19 mm 25.0 162.5 2.4
    0.2 ~ 0.34 mm 28.0 225.0 1.6
    0.35 ~ 1.0 mm 30.0 250.0 1.6
    1.1 ~ 2.5 mm 27.5 225.0 1.6
    2.6 ~ 3.0 mm 26.3 187.5 2.0
    waya mai sanyi
    0.1 mm 6.3 50 6.4
    Bar
    8-100 mm 25 100 3.2

     

    Yanayin maganin zafi
    Kafofin yada labarai masu ratsa zuciya Matsakaici tare da ragowar matsa lamba wanda bai wuce 0.1Pa ba, hydrogen tare da raɓan raɓa wanda bai wuce 40ºC ba.
    The dumama zafin jiki da kuma kudi 1100 ~ 1150ºC
    Rike lokaci 3 ~ 6
    Yawan sanyaya Tare da 100 ~ 200 ºC / h sanyaya zuwa 600 ºC, da sauri sanyaya zuwa 300ºC