Bayanin samfurin
Wadannan an yi amfani da wayoyi masu tasowa don ingantaccen tsayayya, motoci
sassa, iska mai tsayayya da tsayayya, da sauransu ta amfani da rufin rufin da ya dace da waɗannan aikace-aikacen, suna ɗaukar cikakken amfani da bambance-bambancen sifofin enamel shafi.
Bugu da ƙari, zamu aiwatar da rufin enamel mai rufi na waya mai daraja kamar wayar azurfa da waya planinum akan tsari. Da fatan za a yi amfani da wannan samarwa.
Ttpye na rufi:
1) Jerrancearancin Polyester Waya, Class 130
2) Gyara tsayayya da Polyester Volyester Waya, Class 155
3) Jarumar Jeryesimeride Waya Waya, Class 180
4) Polyester (IMID) mai rufi tare da polyamide-lodide juriya na polyamai, aji 200
5) poyimide juriya waya, aji 220
Tpye na waya
nau'in kayan | Cuni1 | Cuni2 | Cuni6 | Cuni8 | Cuni10 | Cuni14 | Cuni19 | Cuni23 | Cuni30 | CUN34 | Cun44 | |
sabbinna | Ni | 1 | 2 | 6 | 8 | 10 | 14.2 | 19 | 23 | 30 | 34 | 44 |
MN | / | / | / | / | / | 0.3 | 0.5 | 0.5 | 1.0 | 1.0 | 1.0 | |
CU | hutu | hutu | hutu | hutu | hutu | hutu | hutu | hutu | hutu | hutu | hutu | |
max aiki | / | 200 | 220 | 250 | 250 | 300 | 300 | 300 | 350 | 350 | 400 | |
denenity g / cm3 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | |
jure wa A 20 ° C | 0.03 ± 10% | 0.05 ± 10% | 0.10 ± 10% | 0.12 ± 10% | 0.15 ± 10% | 0.20 ± 5% | 0.25 ± 5% | 0.30 ± 5% | 0.35 ± 5% | 0.40 ± 5% | 0.49 ± 5% | |
zazzabi | <100 | <120 | <60 | <57 | <50 | <38 | <25 | <16 | <10 | -0 | <-6 | |
tensilesrengengrength MPa | > 210 | > 220 | > 250 | > 270 | > 290 | > 310 | > 340 | > 350 | > 400 | > 400 | > 420 | |
elongation | > 25 | > 25 | > 25 | > 25 | > 25 | > 25 | > 25 | > 25 | > 25 | > 25 | > 25 | |
meltingpoint ° C | 1085 | 1090 | 1095 | 1097 | 1100 | 1115 | 1135 | 1150 | 1170 | 1180 | 1280 | |
tsari mai kyau | 145 | 130 | 92 | 75 | 59 | 48 | 38 | 33 | 27 | 25 | 23 |