Barka da zuwa gidajen yanar gizon mu!

Constantan CuNi44Mn1 Copper Nickel Waya 0.6mm don Dumama Wayoyin

Takaitaccen Bayani:


  • Daraja:KuNi44Mn1
  • Siffar:0.6mm ku
  • Nau'in:Waya
  • Abun ciki:Ku-Ni-Mn
  • Aikace-aikace:Wayoyi masu dumama
  • Cikakken Bayani

    FAQ

    Tags samfurin

    taƙaitaccen gabatarwar samfur

    Constantan Konstantan CuNi44Mn1 Copper Nickel waya 0.6mm don dumama wayoyi.

     

    Tankii Alloys shi ne jan ƙarfe - nickel gami (CuNi44Mn1 gami) wanda ke da ƙarfin juriya na lantarki, babban ductility da kyakkyawan juriya na lalata. Ya dace don amfani a yanayin zafi har zuwa 400 ° C. Aikace-aikace na yau da kullun don Tankii Alloys sune zafin jiki - tsayayyun potentiometers, rheostats masana'antu da juriya na injin motar lantarki.
    Haɗuwa da ƙarancin zafin jiki mara ƙarancin ƙarfi da tsayayyar ƙima yana sa gami da dacewa musamman don jujjuyawar madaidaicin juzu'i.
    Alloys an ƙera su daga electrolytic jan ƙarfe da kuma nickel zalla ta Tankii Co.Ltd, gami da aka keɓe kuma ana samun su da yawa masu girma dabam.

    Na yau da kullun%

     

    Abun ciki
    Abun ciki
    Nickel
    45
    Manganese
    1
    Copper
    Bal.

     

    Kaddarorin injiniyoyi na yau da kullun (1.0mm)

     

    Dukiya Daraja
    Ƙarfin Haɓaka (Mpa) 250
    Ƙarfin Tensile (Mpa) 420
    Tsawaitawa (%) 25

     

    Abubuwan dabi'un Jiki na yau da kullun

     

    Dukiya Daraja
    Yawan yawa (g/cm3) 8.9
    Ƙarfin wutar lantarki a 20 ℃ (Ωmm²/m) 0.49
    Yanayin zafin jiki na resistivity (20 ℃ ~ 600 ℃) X10⁻⁵/℃ -6
    Coefficient na aiki a 20 ℃ (WmK) 23
    EMF vs Cu (μV/℃ )(0~100℃) -43

     

    Coefficient na thermal fadadawa

     

    Yanayin Zazzabi Thermal Fadada x10⁻⁶/K
    20 ℃ - 400 ℃ 15

     

    Ƙaƙƙarfan ƙarfin zafi

     

    Zazzabi Darajar (J/gK)
    20 ℃ 0.41

     

    Wurin narkewa (℃)|1280|

    |Max ci gaba da zafin jiki a cikin iska (℃)|400|
    | Kaddarorin Magnetic | Ba – Magnetic |

    Alloys - Ayyukan Muhalli na Aiki

     

    Alloy Name Aiki A cikin yanayi a 20 ℃ Yin aiki a max zazzabi 200 ℃ (Air da oxygen sun ƙunshi gas) Yin aiki a max zazzabi 200 ℃ (gas da Nitrogen) Yin aiki a max zazzabi 200 ℃ (gases tare da sulfur - oxidability) Aiki a max zazzabi 200 ℃ (gases tare da sulfur - reductibility) Yin aiki a max zazzabi 200 ℃ (carburization)
    Tanki Alloys mai kyau mai kyau mai kyau mai kyau mara kyau mai kyau

     

    Salon Kawowa

     

    Sunan Alloys Nau'in Girma
    Tanki Alloys-W Waya D = 0.02mm ~ 1mm
    Tanki Alloys-R Ribbon W = 0.4 ~ 40, T = 0.03 ~ 2.9mm
    Tanki Alloys-S Tari W = 8 ~ 200mm, T = 0.1 ~ 3.0
    Tanki Alloys-F Tsaye W = 6 ~ 120mm, T = 0.003 ~ 0.1
    Tanki Alloys-B Bar Dia = 8 ~ 100mm, L = 50 ~ 1000