Bayanin samfurin
Wadannan an yi amfani da wayoyi masu tasowa don ingantaccen tsayayya, motoci
sassa, iska mai tsayayya da tsayayya, da sauransu ta amfani da rufin rufin da ya dace da waɗannan aikace-aikacen, suna ɗaukar cikakken amfani da bambance-bambancen sifofin enamel shafi.
Bugu da ƙari, zamu aiwatar da rufin enamel mai rufi na waya mai daraja kamar wayar azurfa da waya planinum akan tsari. Da fatan za a yi amfani da wannan samarwa.
Nau'in Boney Wire
Alloy zamu iya enamelled sune tagulla-nickel alloy waya, Constantan waya, Mangenin waya. Kama waya, NicR Alloy Wire, fecral alloy waya da sauransu
Nau'in rufin
Sunan da aka sanya sunan-enamelled | Matakin thermal ºº (lokacin aiki 2000h) | Sunan Code | Lambar GB | Anssi. Iri |
Polyurethane enamelled waya | 130 | Uew | QA | Mw75C |
Polyester enamelled waya | 155 | Benci | QZ | Mw5c |
Polyester-masu kai tsaye enamelled waya | 180 | Eiw | Da da kullum | Mw30c |
Polyester-Imside da Polyamai-Oride mai cike da rufi mai launi | 200 | Eiwh (Dfwf) | Qy / xy | Mw35c |
Polyamide-imde enamelled waya waya | 220 | Aiw | Qxy | Mw81C |
Cu | Bi | Sb | As | Fe | Ni | Pb | S | Zn | Umarnin rohs | |||
Cd | Pb | Hg | Cr | |||||||||
99.90 | 0.001 | 0.002 | 0.002 | 0.005 | - | 0.005 | 0.005 | - | ND | ND | ND | ND |
Maɗaukaki | 1083ºC |
Melting Point - SULUSS | 1065ºC |
Yawa | 8.91 gm / cm3 @ 20 ºC |
Takamaiman nauyi | 8.91 |
Tsokar lantarki | 1.71 microhm-cm @ 20 ºC |
Harkokin lantarki ** | 0.591 megasemens / cm @ 20 ºC |
A halin da ake yi na thereral | 391.1 W / ME Ok a 20 c |
Madaidaitan yaduwar zafi | 16.9 · 10-6perCºC (20-100 ºC) |
Madaidaitan yaduwar zafi | 17.3 · 10-6perºC (20-200 ºC) |
Madaidaitan yaduwar zafi | 17.6 · 10-6peract (20-300 ºC) |
Takamaiman ƙarfin zafi | 393.5 J / kg ok a 293 k |
Modulus na elalation A cikin tashin hankali | 117000 MPA |
Modulus na tsayayyen | 44130 MPa |